Li, B., Du, X., Shen, Y., Zhang, Z., & Rong, T. (2022). Nonisothermal Crystallization, Growth, and Shape Control of Magnetite Crystals in Molten Nickel Slag During Continuous Cooling. Metallurgical & Materials Transactions. Part B, 53(3), 1816-1826. https://doi.org/10.1007/s11663-022-02491-9
Chicago Style (17th ed.) CitationLi, Bin, Xueyan Du, Yingying Shen, Zhilong Zhang, and Taolin Rong. "Nonisothermal Crystallization, Growth, and Shape Control of Magnetite Crystals in Molten Nickel Slag During Continuous Cooling." Metallurgical & Materials Transactions. Part B 53, no. 3 (2022): 1816-1826. https://doi.org/10.1007/s11663-022-02491-9.