1Academic Journal
Authors: Qiang Tian, Wenwen Zhang, Hucheng Li, Yunlong Liu, Tonggang Lu, Jinhui Du, Xingang Liu, Kaiyao Wang
Source: Journal of Materials Research and Technology, Vol 35, Iss , Pp 4352-4367 (2025)
Subject Terms: GH4742 superalloy, γ′ precipitate, Serrated grain boundary, Fan-type γ′ structure, Cooling rates, Mining engineering. Metallurgy, TN1-997
File Description: electronic resource
Relation: http://www.sciencedirect.com/science/article/pii/S2238785425003540; https://doaj.org/toc/2238-7854
-
2Academic Journal
Authors: Qiang Tian, Wenwen Zhang, Jinhui Du, Tonggang Lu, Yunlong Liu, Xingang Liu, Hucheng Li, Kaiyao Wang
Source: Journal of Materials Research and Technology, Vol 32, Iss , Pp 4198-4211 (2024)
Subject Terms: GH4742 superalloy, γ′ precipitates, Coarsening model, Morphology evolution, Sub-solvus heat treatment, Super-solvus heat treatment, Mining engineering. Metallurgy, TN1-997
File Description: electronic resource
Relation: http://www.sciencedirect.com/science/article/pii/S2238785424020349; https://doaj.org/toc/2238-7854
-
3Academic Journal
Authors: Shulei Yang, Qiang Tian, Ping Yu, Shufeng Yang, Wei Liu, Jingshe Li
Source: Journal of Materials Research and Technology, Vol 24, Iss , Pp 2828-2838 (2023)
Subject Terms: Vacuum arc remelting, GH4742 superalloy, Numerical simulation, Freckle, Mining engineering. Metallurgy, TN1-997
File Description: electronic resource
Relation: http://www.sciencedirect.com/science/article/pii/S2238785423006488; https://doaj.org/toc/2238-7854
-
4Academic Journal
Authors: Wenwen Zhang, Xingang Liu, Qiang Du, Ying Guo, Heyong Qin, Qiang Tian, Mengying Zhu
Source: Journal of Materials Research and Technology, Vol 23, Iss , Pp 13-35 (2023)
Subject Terms: GH4742 superalloy, Sub-solvus heat treatment, Super-solvus heat treatment, γ′ precipitates, Dynamic recrystallization, γ+γ′ duplex structures, Mining engineering. Metallurgy, TN1-997
File Description: electronic resource
Relation: http://www.sciencedirect.com/science/article/pii/S2238785422020841; https://doaj.org/toc/2238-7854
-
5Academic Journal
This result is not displayed to guests.
Login for full access. -
6Academic Journal
This result is not displayed to guests.
Login for full access. -
7Academic Journal
This result is not displayed to guests.
Login for full access. -
8Academic Journal
This result is not displayed to guests.
Login for full access.